01 COA & batch testing

What a chitosan COA reports: deacetylation, viscosity and limits

Technical document 01 · Reviewed 2026-11-19 · Chitosan

On this page
  1. The certificate as a test report
  2. Deacetylation is a ratio; viscosity is a measurement with conditions
  3. Release limit versus batch result
  4. What moves between batches
  5. When to order an outside test
  6. What to compare between suppliers

The certificate for a chitosan lot reports degree of deacetylation by titration, viscosity in 1% acetic acid, moisture, ash, insoluble matter, the heavy-metal panel, microbiology and particle size. There is no single assay percentage, because chitosan is a polymer defined by two properties rather than by one purity figure. The limits in the first table are the catalog specification; the batch COA is the document that confirms a particular pack.

In one line

A chitosan certificate is read on two axes, deacetylation and viscosity; moisture, ash and insoluble matter explain why two lots with the same headline numbers can still behave differently.

The certificate as a test report

A certificate is useful when it can be audited line by line: what was measured, which method produced the number, and which limit the lot was released against. A line that says only “conforms” asks the reader to trust a conclusion without the evidence.

Identity, deacetylation, viscosity and contaminants · chitosan
ParameterMethodRelease limit
AppearanceVisualOff-white to pale yellow powder or flakes
Degree of deacetylationTitration, method named on the certificate≥85%
ViscosityViscometry, 1% in 1% acetic acid50–200 mPa·s
MoistureGravimetric≤10.0%
AshGravimetric after ignition≤1.0%
Insoluble matterDissolution in dilute acetic acid, filtration, gravimetry≤1.0%
Heavy metalsICP-MSPb ≤3 · As ≤2 · Cd ≤1 · Hg ≤0.1 mg/kg
MicrobiologyPlate count and absence testsAPC ≤1,000 cfu/g; yeast and mould ≤100 cfu/g; E. coli and Salmonella absent
Particle sizeSieve analysis≥95% through 80 mesh

Deacetylation is a ratio; viscosity is a measurement with conditions

Degree of deacetylation is the share of glucosamine units that carry a free amine instead of an acetyl group. It is a ratio between repeat units, so it is not corrected to a dried basis the way a small-molecule assay is; moisture does not explain away a low figure. The method does matter. Potentiometric back-titration of the free amine after dissolution in excess acid is the usual approach, proton NMR is the reference method, and an FTIR band ratio is a rapid screen. The same lot can read a few points apart under two methods, so the certificate has to name the one it used.

Viscosity is a property of the solution, not of the powder alone. The catalog figure is measured at 1% in 1% acetic acid, and the reading moves with temperature, spindle, stirring rate and the time the solution stood before it was measured. Chitosan solutions lose viscosity as the chains shorten, so a reading taken after one hour and a reading taken the next day are different measurements. A specification that says “50–200 mPa·s” without the concentration, solvent, temperature and standing time has not fixed the test.

Moisture, ash and insoluble matter are mass fractions of the powder as received, so they are read against the as-is weight. Ash is what remains after ignition: residual mineral from the source and the process, mainly calcium salts and sodium chloride. Insoluble matter is what does not dissolve in dilute acetic acid, usually residual chitin or foreign particulate. Both are small numbers with a large diagnostic value.

Release limit versus batch result

The release limit is the acceptance boundary for the lot; the batch result is what the laboratory measured. Both belong on the page, in separate columns, with the method beside them. A result column filled with the specification range is a copy of the gate, not a result.

What the result column should contain
ParameterRelease limitResult column
Degree of deacetylation≥85%A measured percentage, with the titration method
Viscosity50–200 mPa·sThe measured figure, plus concentration, solvent, temperature and standing time
Moisture≤10.0%A measured percentage
Ash≤1.0%A measured percentage
Insoluble matter≤1.0%A measured percentage, with the dissolution solvent
Heavy metalsPer elementA measured figure in mg/kg for each element
MicrobiologyCounts and absenceThe count and the absence statement for the lot

The viscosity line deserves a second value: the measured figure and the conditions. A number near the top of the range from a solution read after two hours is not the same evidence as the same number read after 24 hours.

What moves between batches

Batch variation in chitosan starts at the deacetylation step and continues through everything after it. Alkali concentration, temperature and hold time set the degree of deacetylation; the same conditions also shorten the polymer chain, so a push towards a higher deacetylation figure usually costs viscosity. The two numbers are linked, and a specification that fixes both narrows the process window the supplier has to work in.

Demineralisation controls ash, filtration and washing control insoluble matter, and drying or bleaching controls colour. Colour is the least quantitative line on the certificate. Off-white to pale yellow is a wide window, and a pink or brown cast can point to residual protein, an oxidation product or a different drying step while deacetylation and viscosity still pass. Ask for the process record before rejecting on shade alone.

Read the trend across lots, not one result near a limit: deacetylation drifting towards 85%, viscosity drifting upward, ash climbing after a source change. Each is a signal to look at the process, not only the number.

When to order an outside test

Order an independent test for a new source, a first shipment into a regulated market, a disputed deacetylation figure, or a viscosity result that cannot be reproduced. The useful panel is not a full repeat: it is titration by a named method plus proton NMR for deacetylation, viscometry under the contract conditions on a freshly prepared solution, ash, insoluble matter, moisture, ICP-MS for the heavy-metal panel and microbiology.

Add a source check when the allergen statement rests on it. Shellfish-derived chitosan carries a crustacean declaration in many markets; a fungal lot carries a different source record, and the two files are not interchangeable. A “not detected” line without a detection limit is evidence about the method’s sensitivity, not about the lot.

Chain of custody applies. The sample tested should be the retained sample, and the report should name the lot and the pack. When a result is contested, give the referee the retained sample, the supplier’s certificate and the contract specification.

What to compare between suppliers

Put six lines side by side: source and CAS number; deacetylation result with the method; viscosity result with the concentration, solvent, temperature and standing time; moisture, ash and insoluble matter; heavy metals and microbiology; pack size and lot code. Two quotations that agree on deacetylation but differ on viscosity or source are not describing the same powder.

The second layer is traceability. The certificate should name who manufactured the lot, which shell or fermentation source was used, and which demineralisation, deacetylation and milling steps were applied. The catalog specification sits on the chitosan product page. The grades page explains how the two headline numbers are traded; the identity page gives the tests that separate chitosan from chitin; the analytical methods describe the instruments behind each row; the release workflow is on the quality page.

Send the specification you intend to use — grade, quantity and destination market — and we will reply with the batch COA, the technical data sheet and a quotation.