01 COA & batch testing

What the chromium nicotinate certificate has to show

Technical document 01 · Reviewed 2026-11-19 · Chromium Nicotinate

On this page
  1. The certificate as a test report
  2. The assay basis and the chromium arithmetic
  3. Release limit versus batch result
  4. What moves between batches
  5. When to order an outside test
  6. What to compare between suppliers

A chromium nicotinate certificate reports appearance, identification by infrared and HPLC, the complex assay by HPLC, chromium by complexometric titration, loss on drying, particle size, the heavy-metal panel and microbiology. Each line needs its method and its release limit, and the batch result belongs in a column of its own. The chromium figure is 12.0–12.8% and the assay is 98.0–102.0%; they are separate gates on the same lot, not two ways of writing one number.

In one line

The certificate has to show two numbers and one ligand: chromium by titration, the complex by HPLC, and an infrared spectrum that names the nicotinate.

The certificate as a test report

A certificate is auditable when every row names the test, the method and the limit the lot was released against. A row that says only “conforms” asks the reader to accept a conclusion without the evidence behind it. Three rows carry the identity of this material: the infrared and HPLC identification, the complex assay and the chromium figure.

Chromium nicotinate is a chromium(III) coordination complex with three nicotinate ligands, formula C18H12CrN3O6 and CAS 64452-96-6. Infrared and HPLC see the ligand from different directions: the spectrum is compared with a reference, while the chromatogram places the nicotinic acid at its own retention time. Neither test is a purity assay, and neither is a substitute for the chromium figure.

Identity, assay and physical limits · chromium nicotinate
ParameterMethodRelease limit
AppearanceVisualGrey-green, free-flowing powder
IdentificationIR and HPLCConforms to reference
Assay (complex)HPLC98.0–102.0%
Chromium (Cr)Complexometric titration12.0–12.8%
Loss on dryingGravimetric≤1.0%
Heavy metalsICP-MSPb ≤3 · As ≤2 · Cd ≤1 · Hg ≤0.1 mg/kg
MicrobiologyPlate count and absence testsAPC ≤1,000 cfu/g; yeast and mould ≤100 cfu/g; E. coli and Salmonella absent
Particle sizeSieve analysis≥95% through 40 mesh

The limits above are the catalog specification. The lot certificate is the document that shows a particular drum met them, and the lot code on the certificate has to match the pouch, the drum and the retained sample.

The assay basis and the chromium arithmetic

The certificate should state whether the 98.0–102.0% assay is calculated on the powder as received or on the dried basis. With a 1.0% loss-on-drying ceiling the two bases differ by at most about one percentage point; it is still a different number, and the basis belongs in the assay row rather than in a footnote.

The chromium line can be checked against the formula. Three nicotinate ligands and one chromium atom give a theoretical chromium content of 12.43%. A complex at 98.0% assay carries about 12.18% chromium, and one at 102.0% carries about 12.68%. The 12.0–12.8% catalog window brackets that arithmetic, which is why the two numbers are read together: a chromium result near an edge with an assay in the middle deserves a question, and a chromium result outside the window with a normal assay points to a second chromium source, a dilution or a calculation error.

The methods are not interchangeable. Complexometric titration measures the metal after the sample is prepared; it does not see the ligand. The ligand evidence is the infrared spectrum and the HPLC result, so a certificate that reports chromium but no ligand line has measured a metal content, not a named complex.

Release limit versus batch result

The release limit is the boundary the lot was accepted against; the batch result is what the laboratory measured. Both belong on the page, in separate columns, with the method beside them. A result column filled with the specification range is not a result; it is the gate copied across.

The lines are not all the same shape. Assay and chromium are windows, loss on drying and the heavy-metal limits are ceilings, identification is pass or fail, and the microbiological lines combine a count with an absence statement. The certificate should keep those shapes rather than turning every parameter into a range.

What the result column should carry · chromium nicotinate
ParameterRelease limitResult column
Assay98.0–102.0%The measured percentage and its basis
Chromium12.0–12.8%The measured percentage and the titration method
Loss on drying≤1.0%The measured percentage
Heavy metalsPer elementA figure in mg/kg for each element
MicrobiologyCounts and absenceThe count and the absence statement for the lot
Particle size≥95% through 40 meshThe measured percentage through the sieve

What moves between batches

The reaction, the crystallisation and the drying step move the chromium result and the colour. The specification allows a grey-green powder, which is a wide window; a batch that is noticeably darker, duller or browner can reflect a different drying end-point or a trace of unreacted ligand while the assay still passes. Colour is a reason to read the batch record, not a rejection on its own.

Milling and sieving move the particle-size line without changing the chemistry. A mill change can shift the 40 mesh result while the assay and the chromium figure stay in place, and the flow on a capsule line will move with it.

A trend across lots says more than one result near an edge: chromium drifting low while the assay holds, loss on drying climbing toward the ceiling, or a new peak in the chromatogram. The lot code on the certificate should match the pack, and the retained sample should come from the same lot.

When to order an outside test

Order an independent test for a new source, a first shipment into a regulated market, a disputed result, or a ligand claim that the supplier's certificate does not prove. The useful panel is not a full repeat of the certificate: infrared for the ligand, HPLC for the complex and the nicotinic acid, chromium by ICP-OES as a cross-check on the titration, loss on drying, ICP-MS for the heavy metals, and microbiology.

Ask the laboratory to report its detection limit for every screen it reports as “not detected”. A limit tells the reader what the method could have seen; a bare absence statement does not. Chain of custody matters as well: the sample tested should be the retained sample, and the report should carry the lot code.

What to compare between suppliers

Put six lines side by side: the declared ligand and CAS number; the assay result and its basis; the chromium result and the method; the identification results by infrared and HPLC; loss on drying and particle size; and the pack, the lot code and the traceability from certificate to drum. Two offers that agree on chromium but differ on the ligand are not the same material.

The catalog specification sits on the chromium nicotinate product page. The tests that separate the nicotinate from another chromium source are on the identity page; the market file is on the compliance page; the titration method is described in the complexometric titration note; the release workflow is on the quality page.

Send the specification you intend to use — grade, quantity and destination market — and we will reply with the batch COA, the technical data sheet and a quotation.

Request a quotation